Electrochemical Noise Measurements in ZRA mode make simultaneous measurements of both current and voltage noise. Two identical corrosion specimens are held at the same potential and the current flow between… read more →
Run this test by selecting Experiment>Electrochemical Noise>ZRA Mode Electrochemical Noise from the Framework™ menu bar. This initiates the following sequence of events: Framework creates a runner window, and the ZRA… read more →
Here is a typical dialog box for a ZRA Mode ECN experiment.All of the Setup parameters for the ZRA Mode ECN test have been discussed in the Common Setup Parameters.
Here is the dialog box for the Potentiostatic Mode ECN Test. All of the Setup parameters for the potentiostatic Mode ECN test except Applied Voltage are described in the Common… read more →
An Electrochemical Noise test in potentiostatic mode measures current noise at a fixed electrode-potential. A corrosion specimen is immersed in a solution and its potential (versus a reference electrode) is… read more →
Run this test by selecting Experiment>Electrochemical Noise>Potentiostatic Mode Electrochemical Noise from the Framework™ menu bar. This initiates the following sequence of events: Framework creates a runner window, and the Potentiostatic… read more →
All of the Setup parameters for the Multiplexed ZRA ECN test are discussed in the setup parameters for Multiplexed Experiments.
The multiplexed ZRA-mode ECN test is a high-throughput version of the single-cell test. It is used for the same purpose.
Run this test by selecting Experiment>Electrochemical Noise>Multiplexed ZRA Mode ECN from the Framework™ menu bar. This initiates the following sequence of events: Framework creates a Runner window, and the Multiplexed… read more →
Here is the Setup dialog box for the multiplexed potentiostatic-mode ECN test. All of the Setup parameters for the Multiplexed potentiostatic-mode ECN test have been discussed in either the single-potentiostatic… read more →